How does free expansion become a reaction force?
Use a 120 mm stack, chemical strain coefficient 0.01 per SOC fraction, ΔSOC = 0.5, α = 20×10⁻⁶/K and ΔT = 20 K. Stack and housing stiffnesses are 1000 and 2000 N/mm.
Chemical and thermal eigenstrains specify stress-free growth under the stated additive model. Constraint converts part of that growth into elastic compression and force. If the measured chemical curve already contains the temperature contribution, adding it again double-counts expansion.
Connect the physical quantities
The relationship used in this example
A stress-free expansion is a strain input, whereas gas pressure is a surface traction. They can both deform a cell but enter mechanics differently. A model should define the reference SOC and temperature, identify what its calibrated growth curve already includes, and then apply the surrounding constraints.
Work through the example
SOC contribution is 0.01×0.5 = 0.005; thermal contribution is 20×10⁻⁶×20 = 0.0004.
Multiply their sum by 120 mm to obtain 0.648 mm free growth.
Divide by 1/1000+1/2000 = 0.0015 mm/N to obtain 432 N; verify 432/2000+432/1000 = 0.648 mm.
Full example conditions and reference values
Assume a synthetic linear thickness law with βz = 0.01 per unit SOC fraction, SOC rising from 0.2 to 0.7, αz = 20×10⁻⁶ K⁻¹ and temperature rising by 20 K. Then εz* = 0.0054. For H = 120 mm, free growth is 0.648 mm. With kc = 1000 N/mm and K = 2000 N/mm, no initial preload and no gap, the scalar model gives 432 N, fixture opening 0.216 mm and stack compression relative to the free state 0.432 mm. Gas pressure is not included in this example.
Compare the numbers before judging the result
| Condition | Free strain | Free growth (mm) | Force (N) |
|---|---|---|---|
| Chemical only | 0.005 | 0.6 | 400 |
| Chemical + thermal | 0.0054 | 0.648 | 432 |
Independent additive contributions are assumed; a measured curve already containing thermal expansion must not be counted twice.
What the result means for a model
Record SOC, temperature, pressure and reference thickness with the growth data. An imposed eigenstrain and a gas-pressure load can coexist only with a clear accounting of what each represents; applying both to explain the same measured expansion double-counts the driving mechanism.
Another application: Keep thermal growth from being counted twice
The example adds chemical strain 0.005 to thermal strain 0.0004, giving 0.0054. This addition is meaningful only if the chemical coefficient was identified without already including that temperature-driven growth. A measured total thickness curve may contain both contributions.
Further modeling details
Define the reference state
Zero eigenstrain means no change from a declared reference, not necessarily zero SOC or a new cell. Record SOC0, T0, aging state and preload separately. If the geometry was measured in an already swollen state, applying growth from an unrelated zero can count the same deformation twice.
Choose a scale and direction
Particle insertion strain, electrode expansion and measured cell thickness change are not interchangeable coefficients. A pouch stack can be strongly directional. Use a scalar thickness law only when the output of interest and calibration support that reduction; use a tensor or layered description when lateral constraint and internal stress matter.
Do not double-count physical sources
A measured thickness curve may contain reversible insertion expansion, irreversible growth, temperature effects and gas-induced bulging. Adding an independent gas-pressure load to a curve already containing that response can overpredict deformation. Separate sources experimentally or define a deliberately lumped model with a clear scope.
Make the coupling handoff explicit
In a sequential workflow, transfer SOC or concentration and temperature with units, reference states, locations and times. Interpolate those fields before evaluating the structural law. One-way coupling assumes structural pressure does not materially change the electrochemical solution over the intended range; that assumption requires examination when feedback matters.
Validate more than one observable
Compare free growth first, then force under a known restraint and, if available, spatial thickness or pressure. Agreement in force alone can hide a wrong combination of expansion and stiffness. Use different SOC paths, temperature or restraint states as withheld checks rather than fitting every case separately.
Separate response history before assigning a cause
Use reversible breathing, mechanically residual deformation and aging-related growth as bookkeeping channels, not automatically identifiable measurements. A returned SOC does not guarantee a returned temperature, stress or relaxation state. Define whether thermal expansion is included in breathing or tracked separately. If gas is included in aging growth, do not add it again as a separate thickness contribution.
A two-state thickness example
At matched temperature and reference load, suppose a synthetic cycle starts at 10.000 mm, reaches 10.120 mm at high SOC and returns to 10.030 mm after discharge and a specified rest. The peak-to-rest recovery is 0.090 mm and the remaining offset is 0.030 mm. Calling the offset aging alone is not supported: mechanical residual strain, slow recovery, drift and aging can contribute. Repeat the reference-state measurement and add independent observations.
The same residual can have competing explanations
Two deliberately synthetic allocations, 0.020 mm mechanical + 0.010 mm aging or 0.005 mm mechanical + 0.025 mm aging, both reproduce a 0.030 mm offset. They are arithmetic counterexamples, not identified material states. Longer recovery, changed restraint, reversible cycling and independent electrochemical or imaging evidence can constrain alternatives, but no single test uniquely resolves every mechanism.
Transfer only the quantity the structural model expects
A measured constrained thickness already includes a mechanical response to load. It is not automatically a stress-free eigenstrain. Document the reference geometry, SOC, temperature, aging state, pressure and rest protocol before transferring a free-growth law. If gas is a pressure load, use its mechanical model to predict displacement rather than treating pressure as an additive strain.
Formula and symbol reference
Open the complete formula reference
| Symbol | Meaning | Unit / convention |
|---|---|---|
| ε*, εp | Stress-free eigenstrain and plastic strain in a small-strain split | dimensionless |
| βz, αz | Illustrative thickness strain per SOC fraction; thermal expansion coefficient | dimensionless; 1/K |
| H, kc, K | Stack height and scalar stack/restraint stiffness | mm; N/mm |
| pg, n | Pressure difference and outward structural surface normal for a pressure load | MPa; unit vector |
When this example stops applying
Synthetic linear small-strain demonstration, not a calibrated battery law. No gas generation, electrochemical solver, degradation kinetics or spatial stress solution is computed. Large deformation and anisotropic constitutive identification require additional modeling.
Check your interpretation
Can a measured total thickness-growth curve and an independent gas-expansion load always be added?
Show the reasoning
No. First establish whether gas effects are already included in the measured curve and whether the two contributions share consistent reference states and constraints.
Sources and calculation scope
- Giudici, Chapman & Please (2024) · Mechanical stresses in pouch cells: a reduced order model
- COMSOL 6.2 · Battery Design Module and intercalation strain
- Ipers et al. (2024) · Electro-chemo-mechanical deformation, elastic/plastic/diffusion contributions
The questions and comparison tables are independently authored teaching examples. Numbers illustrate the stated models; they are not measured cell/pack data or commercial-solver validation.
Comparison calculations (Python)