How do mean stress and mixed cycles enter a life estimate?
First correct an 80 MPa amplitude with 100 MPa tensile mean and Su = 400 MPa. Then consider a separate block containing 10000/100000 and 20000/1000000 consumed-life fractions.
Mean-stress correction changes the amplitude used to read a compatible S–N curve. Miner summation then adds consumed fractions using the life assigned to each cycle class. These are two stages; the independent block numbers here are not claimed to come from the first corrected amplitude.
Connect the physical quantities
Mean stress shifts a cycle without changing its amplitude. A mean-stress correction maps that cycle to a reference curve under assumptions. Miner summation then counts fractions of life; it discards sequence effects and is not a model of crack closure or overload retardation.
The relationship used in this example
A variable-amplitude history must be converted into cycles with defined amplitudes and means. Mean-stress correction maps each cycle to the reference curve condition. A cumulative-damage rule then combines the corresponding life fractions.
Work through the example
Goodman denominator is 1−100/400 = 0.75.
Equivalent amplitude is 80/0.75 = 106.667 MPa.
For the separate damage block, 10000/100000 + 20000/1000000 = 0.12; 1/0.12 = 8.333 blocks.
Full example conditions and reference values
For amplitude 80 MPa, tensile mean stress 100 MPa and Su = 400 MPa, the illustrative Goodman correction gives 106.67 MPa. Separately, a block with 10,000 cycles at a level having life 100,000 and 20,000 cycles at a level having life 1,000,000 has D = 0.12; identical repetition predicts 8.33 blocks to nominal D = 1.
Compare the numbers before judging the result
| Repeated blocks | Miner sum D |
|---|---|
| 1 | 0.12 |
| 5 | 0.6 |
| 8 | 0.96 |
D is a model sum, not the probability that the part has failed.
What the result means for a model
The correction becomes ill-conditioned as mean stress approaches tensile strength; this is not a safe extrapolation region. Preserve each cycle mean during Rainflow counting. Treat D = 1 as a model prediction with material and loading uncertainty, not an exact failure clock.
A change in tensile mean stress changes the corrected cycle amplitude before life fractions are added. Keep raw cycle bins, mean-stress treatment and curve version so that the life estimate can be recalculated when the load history changes.
Another application: A damage sum needs a load sequence
The example block has D = 0.12. Five identical blocks give 0.60; eight give 0.96. The nominal 8.33-block prediction assumes the same cycle content and Miner summation. It is not a 60% or 96% probability of failure.
Further modeling details
Cycle counting
Rainflow counting reduces a turning-point history to closed and residual cycles. Sampling rate, filtering and treatment of residual half cycles affect the result. Preserve the original signal and state whether a repeated block was closed or treated as a finite record.
Avoid double correction
A material curve may already represent a particular mean stress, surface or weld condition. Apply corrections consistently with that reference and the selected software method.
What to retain in a report
Save cycle distributions, correction assumptions, damage contributions by load level and the fatigue-critical locations. A single life contour cannot explain which events govern the prediction.
Formula and symbol reference
Open the complete formula reference
| Symbol | Meaning | Unit / convention |
|---|---|---|
| Su | Ultimate tensile strength for illustrative Goodman correction | MPa |
| ni, Ni | Applied cycles; life at the corrected cycle level | cycles |
| D | Miner damage sum | dimensionless |
| B | Identical repeated blocks to nominal D = 1 | blocks |
When this example stops applying
The Goodman expression here assumes tensile mean stress below Su. Compressive-mean treatment is method-dependent. Miner’s rule neglects sequence effects and overload interactions; D = 1 is a model criterion, not a guaranteed test failure point. Fatigue damage D is not the stiffness-degradation variable d.
Check your interpretation
Does Miner’s rule distinguish high–low from low–high load ordering?
Show the reasoning
Not when cycle counts and associated lives are unchanged. That is a limitation of the linear rule.
Sources and calculation scope
The questions and comparison tables are independently authored teaching examples. Numbers illustrate the stated models; they are not measured cell/pack data or commercial-solver validation.
Comparison calculations (Python)
English / Korean · revised 1 November 2026