  "source": "D01",
  "source_doi": "10.1016/j.ijplas.2019.06.011",
  "locator": "Table 2, PDF p.7 / journal p.299",
  "status": "TRANSCRIBED_REFERENCE_ONLY_NOT_MATERIAL_CARD",
  "visual_table_check": true,
  "scope": "electrode coatings, not homogenized pouch cell",
  "anode_graphite": {
    "beta_deg": 60,
    "cohesion_c_MPa": 1.0,
    "cap_R": 0.7
  },
  "cathode_NMC": {
    "beta_deg": 65,
    "cohesion_c_MPa": 4.0,
    "cap_R": 0.8
  },
  "missing": {
    "pa_hardening_curve": null,
    "elastic_modulus": null,
    "poisson_ratio": null,
    "initial_state": null,
    "strain_convention_mapping": null,
    "pa_hardening_curve_note": "Published curve digitized; inelastic strain and initial-state interpretation remain unresolved."
  },
  "mapping_rule": "Abaqus cap hardening uses pb, not pa: pb = pa*(1+R*tan(beta)) + R*d. Confirm stress and inelastic volumetric strain signs and reference before creating a card.",
  "prohibited_use": "Do not fill missing entries with another cell or silently mix Ipers/Deng parameters.",
  "digitized_curve_followup": "dpc-native-v01.html",
  "digitized_pressure_curve_status": "129 points with ordinate mapping; not inelastic hardening card"
}